   Dressing Conditions

 


 

   

What happens when dress "Too Slow"
 
  Grains Too Smooth

  1. Poor cutting action
  2. Chatter marks
  3. Burning & cracks

Dressing Conditions

What happens when dress "Idle Pass"

Sharp points on wheel grains are made blunt

1. Poor cutting action
2. Unevenness (Waviness)

Wheel dressed with a high depth of cut

Grains broken and pulled out


1. Very rough finish
2. Wheel gets loaded too soon

What happens when we dress "Dry"

Grains pulled out due to bond failure

1. Very rough finish
2. Change in ground from & taper
3. Wheel gets loaded

What happens when we dress "Correctly"

1. Sharp edges on grains
2. No cavities

------------------------------------------------------------------------------------------------------------------------------------------------------------------------
   BACKABOUT US  |  OUR  PROFILE |  OUR PRODUCTS |  CONTACT  US  |  FEEDBACK  |  TOPNEXT

| Home | Profile | About Us | Single Point Diamond Dressers | Throw - Away Diamond Dressers | Shaping Tools | Cluster Dressers | Multipoint Indexable Crown | Hexagonal Disc Diamond Dressers | Multipoint Disc | Diamond Grit Impregnated Dressers | Blade Type Dressers | Diamond Indenters | Diamond & C.B.N. Wheels | Diamond & CBN honing stone | Contact Us | Enquiry |

 

 
 

 
 
Designed & Hosted by : MID   Promoted by : GID